by gencboya | Oct 31, 2025 | Paint Defects and Solutions
Dry Spray (Spray Dusting) Issue Problem Description: Dry spray occurs when paint emitted from the spray gun dries too quickly and adheres to the surface in a rough, textured manner. Although this issue may not always be visually obvious, it can be felt by touch. It...
by gencboya | Oct 31, 2025 | Paint Defects and Solutions
Primer Cracking Problem Description: Primer cracking refers to cracks that develop on the primer layer’s surface. These cracks occur due to poor adhesion of the primer or stresses arising during the drying process. Cracking typically results from incompatibility...
by gencboya | Oct 31, 2025 | Paint Defects and Solutions
Sanding Marks Problem Description: Sanding marks are scratches that occur on furniture surfaces during the sanding process. These marks generally result from excessive pressure on the sandpaper, improper choice of sanding material, or incorrect sanding technique....
by gencboya | Oct 31, 2025 | Paint Defects and Solutions
Silicone Blushing (Silicone-Induced Surface Defects) Problem Description: Silicone blushing refers to surface defects such as blistering or peeling caused by volatile substances (often silicone-containing products like perfumes, deodorants) interacting with the paint...
by gencboya | Oct 31, 2025 | Paint Defects and Solutions
Delayed Drying / Incomplete Curing Problem Description: The delayed drying or incomplete curing issue in furniture coatings, particularly with polyurethane, water-based, acrylic, and cellulosic paints, occurs when the paint fails to dry within the expected timeframe...